Worldwide Distributor of Electric Motor Repair & Cathodic Protection Materials Since 1986
State of the art production techniques yield a higher open circuit voltage (driving) potential than conventional H-1 alloy anodes. These anodes produce potentials of 1.75 Volts with a “certified” minimum current efficiency of 50%, allowing protection levels to be achieved using fewer anodes.The chemistry is per ASTM B843 Industry Standard for high potential anodes-Alloy M1C.
Options (Lbs):